Ditemukan 5 dokumen yang sesuai dengan query
Abstrak :
In order to review the structure and characteristic of pressure sensitive label (PSL), the examination of 32 PSL smples has been carried out. The results of visual examination show that PSL is a laminate, consist of label paper layering by adhesive and coated release-paper. The test results showed that the basis weight of PSL is 171.3 - 220.7 g/m2 with the caliper of 0.1680 - 0.2348 mm. The basis weight is correlated well with caliper anfa adhesiveness, but isit not with tensile strength, stretch, and tear strength. The ash content is at least 10 % which means that paper components of PSL contain onorganic filler.
Artikel Jurnal Universitas Indonesia Library
Abstrak :
Treatment of pulp bleaching effluent using Upflow Anaerobic Sludge Blanket (UASB) and Suspended Carrier Biofilm (SCB) systems have been carried out. Upflow Anaerobic Sludge Blanket (UASB) and Suspended Carrier Biofilm (SCB) reactors were run on the Hydraulic. Retention Time (HRT) of 12 hours, respectively. Micronutrient solution containing some traces elements was added into feed wastewater of UASB reactor to accelerate the growth of granular sludge. Sludge characteristics of UASB and activeted sludge reactors were observed and analyzed. Settling rate of granular reactor was also measured. Effluent of UASB reactor was treated further in Susoended Carrier Biofilm (SCB) reactor. Concentration of COD, TSS and AOX parameters both influent and effluent of UASB reactor as well as suspended carrier biofilm (SCB) reactor were analyzed. Result revealed that UASB reactor run on the Hydraulic Retention Time (HRT) of 12 hours could remove COD up to 90 % and AOX up to 84 %. Addition of micronutrient solution has accelerated the growth of granular sludge. Dark-brownesh color of granular sludge with the diameter of 1-4 mm having settling rate of 70-120 m/hr has been formed. SCB reactor as post-treatment could remover COD of 85%, TSS of 73 % and AOX of 76%. Sequential UASB and SCB reactor could increase the effectivity of pulp and paper mill wastewatertreatment with the removal of dissolved and suspended organic pollutant more than 94%.
Artikel Jurnal Universitas Indonesia Library
Abstrak :
Utilization of paper mill sludge from waste treatment plnt for compost have been proven able to improve the quality of land and crop productivity and also uncontaminate the environment. But to produce the compost on a large scale, industry still not yet implemented it because composting process can take time uo to 3 month. Composting of paper mill sludge by fungi Phanerochaeta chrysosporium, Trichoderma harzianum ad Trichoderma reesei have been done atLaboratory scale. The results showed that composting of paper mill sludge by fungsi Treichoderma harzianum have the highest cellulose degradation. Composting process for 28 day, can reach the quality standard of compost.
Artikel Jurnal Universitas Indonesia Library
Abstrak :
Oil spill can contaminate the environment as a consequence of activities related to crude oil exploration, oil refinary, transporation, pipeline leaking, and industrial processes. This researchrelated with the characteristics of coir dust as oil sorbent material to remove oil from water. Hydrophobicity is an important parameter that determines the effectiveness of the oil sorbent. Some treatment were done in this research to increase the hydrophobicity of choir dust. Moreover, these treatments were expected to improve oil sorption capacity of coir dust. They are heating andacetylation prosess. The results showed both of heating and acetylation could increase hydrophobicity and oil sorption capacity onto coir dust.
Artikel Jurnal Universitas Indonesia Library
Abstrak :
In this experiment, xylanase was used prior to bleaching. The dosages of xylanase are 0.25; 0,5; 0,75; 1;1,25 kg/ton of chips. The pulps after pretreatment were tested and treated with D0ED1D2 bleaching sequences. The result shoew that xylanase can decreasekappa number as much as 10.33-11.45. The optinum kappa number (10.33) was obtaidned by addition xylanase 0.75 kg/ton of chips. Xylanase also increases increase bleachability of pulp and decrease dirt on pulp, from initial brightness 82.4 % ISO to 83.10 % ISO. While dirt from 9.5 mm2/m was decrease to 7-8 mm2/m2. Xylanase was able to decrease dichloromethane extractive content in bleached pulp as much as 0.06-0.14 point. Xylanase also increases bleaching selectivity, as physical strength of pulp tend to increase.